2000-4-14 · The AE amplitude were observed to be higher for a harder-bonded material that holds the diamond grits on the wheel surface. For a hard-bond material such as cast iron, the AE amplitude generated from the grinding zone is higher (206) compared with the AE amplitude (116) generated from vitrified bonded wheel.