An Environmentally Friendly Modified Wet-Filament
2011-5-27 · diamond-coated cutting wheel. The mass of the test specimens were measured using a five-digit analytical balance. The “burn-off” tests were carried out in a muffle-furnace at 575 °C for 10 hours. (b) Image analysis Samples of 20 x 20 mm were cut using a diamond-coated wheel and mounted using an epoxy adhesive.